- Interlining -



- Double Dot Fusible -
Suiteable for the frontpiece main-interlining of outer garment, collar front-neckband and small parts of apparel
- Paste Dot Fusible -
- Scatter Powder Fusible -
Apply on from neckband, cuff of fashion apparel or sand-cleaning silk apparel. The grey interlining, spunlace or slit-making interlinings apply on frontpiece men and women garments.
Apply on childern apparel, cotton&bast, leather substrates, chemical fibre apparel and shoe, cap interlinings.
Continual Pressing Machine:
Flat-bed Pressing Machine:
Temp °C
Pressure (Kg/cm2)
Time (sec)
125-150
120-140
1-2
0.8-2
12-18
12-16
Technical Data:
Cleaning Restrictions: Water wash blow 40°C and resist dry cleaning.
Technical Data:
Continual Pressing Machine:
Flat-bed Pressing Machine:
Temp °C
Pressure (Kg/cm2)
Time (sec)
125-140
120-140
1-2
0.5-1
12-18
10-15
Cleaning Restrictions: PA powder interlining - dry clean.
PES powder interlining - water-washing, sand- cleaning.
EVAL powder interlining - water-washing.
Technical Data:
Continual Pressing Machine:
Temp °C
Pressure (Kg/cm2)
Time (sec)
100-120
0.5-1
10-15
Cleaning Restrictions: EVA powder interlining can't resist either dry clean or water washed.
EVAL powder interlining - water-washing.
LDPE powder interlining - water-washing.









- Western-style Interlining -
Technical Data:
Cleaning Restrictions: Water wash blow 40°C and resist dry cleaning.
Continual Pressing Machine:
Flat-bed Pressing Machine:
Temp °C
Pressure (Kg/cm2)
Time (sec)
125-140
130-150
1-2
0.8-2
12-18
12-16


- Jacket Interlining -
Technical Data:
Cleaning Restrictions: Water wash blow 40°C and resist dry cleaning.
Continual Pressing Machine:
Flat-bed Pressing Machine:
Temp °C
Pressure (Kg/cm2)
Time (sec)
125-140
130-150
1-2
0.8-2
12-18
12-16